Need some help guys, or to whoever has done the badges before, :help:
am i doing it wrong or something ? because its not turning out the way i wanted to,
here are the photos:
Started off with a brand new chrome badge all cleaned and off the grille
First coating done, dried it for about 1 hr, (can said 30 mins but i did an hour cos i was playing games )
also i did this on a flat surface (horizontal)
Did two coats for this one, didnt really take another shot because it looks exactly like the 1st one all shiny, waited another hour to dry and it ended up looking like this ....
Okayyy.. so then it obviously doesnt look proper at all, so i took my old one that has been sanded down with the chrome bits off with 400 paper, and also sprayed this vertically, (thought it wouldve made a difference) that was also the 1st coat and dried for also an hour.
Here is the comparison between the two,
left one was the 1st one sprayed horizontally (not that it makes a difference i think) 2 coats.
right one was vertically, but only sprayed with one. and it almost has the simillar effects even though its been sanded down.
Now the can said do 3-4 coats, i stopped at 2 coats to avoid what maybe a waste.
Here is the result of the 2nd badge (sanded one done vertically) after the second coat. I stopped again as soon as those little grooves and cracks showed up.
Questions come to my mind.
-am i drying it for too long ?
-should i be spraying only 1 coat ?
-is there some sort of primer im supposed to use?
*and many more but only these are what i could think of as i type this*
ive been looking at the pics at the plastidip thread and mine doesnt look like anything compared to those ones :(
Any help/opinions/suggestions would be great. :D
Thanks all !
-jeffy :]